Description

Filament test sample – CzechPrint3D

A small test strip (80 × 10 × 3.4 mm) with an embossed CP3D logo lets you assess the material before buying a full spool. Feel the surface, bend it in your hands, check its flexibility, strength or brittleness and judge how it will behave in practice.

All printed with the standard Bambu Lab profile or on a Prusa HT90.

The sample colour is random – it shows the material's properties, not the shade.

Technical data

Product lineBambu Lab ASA
AMSAMS (not AMS lite)
Enclosed printerRecommended

Recommended print settings

Drying before printingBlast Drying Oven: 80 °C, 8 h X1 Series Printer Heatbed: 90–100 °C, 12 h
Printing and storage humidity< 20% RH (Sealed, with desiccant)
Nozzle size0.2, 0.4, 0.6, 0.8 mm
Nozzle temperature240–270 °C
Plate preparationGlue
Bed temperature80–100 °C
Cooling fan0–80%
Print speed< 250 mm/s
Chamber temperature45–60 °C

Physical and mechanical properties

ValueMethod
physical
Density1.05 g/cm³ISO 1183
Melt index7.0 ± 0.8 g/10 min260 °C, 2.16 kg
Melting temperature210 °CDSC, 10 °C/min
Vicat softening temperature106 °CISO 306, GB/T 1633
Heat deflection temperature 1.8 MPa92 °CISO 75 1.8 MPa
Heat deflection temperature 0.45 MPa100 °CISO 75 0.45 MPa
Water absorption0.45%25 °C, 55% RH
mechanical
Young's modulus (X‑Y)2450 ± 270 MPaISO 527, GB/T 1040
Young's modulus (Z)2120 ± 260 MPAISO 527, GB/T 1040
Tensile strength (X‑Y)37 ± 3 MPaISO 527, GB/T 1040
Tensile strength (Z)31 ± 4 MPaISO 527, GB/T 1040
Elongation at break (X‑Y)9.2 ± 1.4 %ISO 527, GB/T 1040
Elongation at break (Z)4.6 ± 0.8 %ISO 527, GB/T 1040
Bending modulus (X‑Y)1920 ± 130 MPaISO 178, GB/T 9341
Bending modulus (Z)1650 ± 120 MPaISO 178, GB/T 9341
Bending strength (X‑Y)65 ± 5 MPaISO 178, GB/T 9341
Bending strength (Z)40 ± 3 MPaISO 178, GB/T 9341
Impact strength (X‑Y)41.0 ± 2.3 kJ/m²; 19.6 ± 1.8 kJ/m² (notched)ISO 179, GB/T 1043
Impact strength (Z)4.9 ± 0.6 kJ/m²ISO 179, GB/T 1043

Downloads

Manufacturer data from Bambu Lab, standard test specimens. For comparison only; actual part properties depend on the printer and settings.