Vzorek - PLA Wood
CZK 10
We are not VAT registered; prices are final.
Delivery and pickup
Packeta pickup point CZK 89, home delivery CZK 119, express courier in Prague by arrangement CZK 500, pickup in Prague 5 free. Cash on delivery +CZK 30. Free delivery in Czechia from CZK 3,000. Slovakia CZK 119 (pickup point) / CZK 159 (address); we do not ship goods to other countries.
Not sure about the material? Ask for a free test sample with your order.
Description
Filament test sample – CzechPrint3D
A small test strip (80 × 10 × 3.4 mm) with an embossed CP3D logo lets you assess the material before buying a full spool. Feel the surface, bend it in your hands, check its flexibility, strength or brittleness and judge how it will behave in practice.
All printed with the standard Bambu Lab profile or on a Prusa HT90.
The sample colour is random – it shows the material's properties, not the shade.
Technical data
| Product line | Bambu Lab PLA Wood |
|---|---|
| AMS | AMS and AMS lite |
| Enclosed printer | Not needed |
Recommended print settings
| Drying before printing | Blast Drying Oven: 55 °C, 8 h X1 Series Printer Heatbed: 65–75 °C, 12 h |
|---|---|
| Printing and storage humidity | < 20% RH (Sealed, with desiccant) |
| Nozzle size | 0.4, 0.6, 0.8 mm |
| Nozzle temperature | 190–240 °C |
| Build plate | Textured PEI Plate / Smooth PEI Plate |
| Plate preparation | Glue |
| Bed temperature | 35–45 °C |
| Cooling fan | Turn on |
| Print speed | < 250 mm/s |
| Chamber temperature | 25–45 °C |
| Support material | Support for PLA |
Physical and mechanical properties
| Value | Method | |
|---|---|---|
| physical | ||
| Density | 1.21 g/cm³ | ISO 1183 |
| Melt index | 29.4 ± 1.7 g/10 min | 210 °C, 2.16 kg |
| Melting temperature | 156 °C | DSC, 10 °C/min |
| Glass transition temperature | 54 °C | DSC, 10 °C/min |
| Vicat softening temperature | 64 °C | ISO 306, GB/T 1633 |
| Heat deflection temperature 1.8 MPa | 57 °C | ISO 75 1.8 MPa |
| Heat deflection temperature 0.45 MPa | 60 °C | ISO 75 0.45 MPa |
| Water absorption | 1.25% | 25 °C, 55% RH |
| mechanical | ||
| Young's modulus (X‑Y) | 2360 ± 190 MPa | ISO 527, GB/T 1040 |
| Young's modulus (Z) | 1770 ± 150 MPa | ISO 527, GB/T 1040 |
| Tensile strength (X‑Y) | 26 ± 5 MPa | ISO 527, GB/T 1040 |
| Tensile strength (Z) | 15 ± 4 MPa | ISO 527, GB/T 1040 |
| Elongation at break (X‑Y) | 15.3 ± 3.1 % | ISO 527, GB/T 1040 |
| Elongation at break (Z) | 4.5 ± 1.7 % | ISO 527, GB/T 1040 |
| Bending modulus (X‑Y) | 2780 ± 120 MPa | ISO 178, GB/T 9341 |
| Bending modulus (Z) | 1975 ± 140 MPa | ISO 178, GB/T 9341 |
| Bending strength (X‑Y) | 55 ± 4 MPa | ISO 178, GB/T 9341 |
| Bending strength (Z) | 28 ± 4 MPa | ISO 178, GB/T 9341 |
| Impact strength (X‑Y) | 15.7 ± 3.7 kJ/m²; 6.3 ± 2.2 kJ/m² (notched) | ISO 179, GB/T 1043 |
| Impact strength (Z) | 5.6 ± 1.2 kJ/m² | ISO 179, GB/T 1043 |
Downloads
Manufacturer data from Bambu Lab, standard test specimens. For comparison only; actual part properties depend on the printer and settings.